TC17titaniumalloy alloy after quenching and aging dagger step reinforcement, strength at room temperature can reach 1372-1666 MPa;But, the poor thermal stability should not be used at high temperature.

TC17 titanium alloy chemical composition
| 
			 Grade  | 
			
			 Main components% %  | 
			
			 impurity /%,Not more than  | 
		|||||||||
| 
			 AL  | 
			
			 Mo  | 
			
			 Mn  | 
			
			 Sn  | 
			
			 Fe  | 
			
			 C  | 
			
			 N  | 
			
			 H  | 
			
			 O  | 
			
			 other  | 
		||
| 
			 single  | 
			
			 total  | 
		||||||||||
| 
			 TC17  | 
			
			 4.4~5.5  | 
			
			 3.5~4.5  | 
			
			 1.5~2.5  | 
			
			 1.5-2.5  | 
			
			 0.15~0.3  | 
			
			 0.05  | 
			
			 0.05  | 
			
			 0.05  | 
			
			 0.10  | 
			
			 0.10  | 
			
			 0.30 
  | 
		